What materials do I need to make a mould?
What materials do I need to make a mould?
Post Reply
Like
2
What materials do I need to make a mould?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jozi
Jozi
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 18,
Visits: 60
I'm new to this and was about to go out and pay for the
EC Epoxy mould starter kit
but I'm not sure it's what I want!
I think I'd prefer to work with fibreglass for making a mould as I'm not sure the epoxy kit gives me enough materials to make a mould.
Could someone help me put together a list of material to buy so I can get started making a fg mould?
Reply
Like
2
Reply
440CUDA
440CUDA
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Awaiting Activation
Posts: 3,
Visits: 11
http://www.fibreglast.com/fibreglast_how_to_make_fiberglass_mold
I hope this helps you out.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
What materials do I need to make a mould?
Jozi
-
12 Years Ago
http://www.fibreglast.com/fibreglast_how_to_make_fiberglass_mold I hope this helps you out.
440CUDA
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search