wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
Making some large Moulds ( 2.5m x 2.5m ) at the moment and this unusually hot weather is really slowing me down. Even at .75% I can only mix 5-600grms of resin at a time, giving me about 10 minutes before the stuff starts to gel in the pot. I have now started mixing 4 or 5 batches in tray like containers and putting them in the fridge before use. This is helping but has anyone else developed any cunning solutions?
Cheers Warren
Carbon
Copies Ltd
Reply
Like
3
Reply
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
what i do is take a painting-tray ,and put a freezerblock under it, then put my pot of resin on top of this and you'll get some precious extra working time
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Issues with the High Temperatures
wozza
-
12 Years Ago
Slow MEKP: http://www.ecfibreglasssupplies.co.uk/p-2490-catalyst-slow-reactivity-mekp.aspx Or...
carboncactus
-
12 Years Ago
[quote][b]carboncactus (18/07/2013)[/b][hr]Slow MEKP:...
wozza
-
12 Years Ago
better do for me infusion i do for you any polyster ;)
TomDesign
-
12 Years Ago
[quote][b]TomDesign (18/07/2013)[/b][hr]better do for me infusion i do for you any polyster...
wozza
-
12 Years Ago
If you're ordering both, order them from CFS. I just linked to East coast for the first one because...
carboncactus
-
12 Years Ago
Send me stuff Warren i do for you good molds and you can do for me infusion as that is still for me...
TomDesign
-
12 Years Ago
what i do is take a painting-tray ,and put a freezerblock under it, then put my pot of resin on top...
matthieutje65
-
12 Years Ago
What about an AC'd workshop?
baja_patient
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search