Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
Meter panel for Hummer 1
Meter panel for Hummer 1
Post Reply
Like
2
Meter panel for Hummer 1
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
shmat_ok (Nikolay)
shmat_ok (Nikolay)
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 101,
Visits: 459
At last that started panel production.
Reply
Like
2
Reply
shmat_ok (Nikolay)
shmat_ok (Nikolay)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 101,
Visits: 459
When took a detail from a matrix, understood that gelcoat was superfluous. it is necessary to peel it and to smooth out.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Meter panel for Hummer 1
shmat_ok (Nikolay)
-
12 Years Ago
After the first layer two layers of CF650 twill and between them coremat soric inserts follow.
shmat_ok (Nikolay)
-
12 Years Ago
we prepare 2,5 kg. Sicomin SR 8100/SD 8822 pitches... ... also it is necessary to wait only
shmat_ok (Nikolay)
-
12 Years Ago
When took a detail from a matrix, understood that gelcoat was superfluous. it is necessary to peel...
shmat_ok (Nikolay)
-
12 Years Ago
RE: Meter panel for Hummer 1
shmat_ok (Nikolay)
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search