Hi there,
I've made a mould to produce Carbon fibre loops, the dimensions of the grooves are 5x5mm, which is the intended cross section dimensions of loops. Initially I had an idea of taking carbon fibre loops out of mould and vacuum bagging them then i realised the might change the square cross section of loops which i want to keep.
So I wonder if vacuum bagging to whole mould with fibres in grooves will be efficient in this case or grooves too small?
And do you recommend any special arrangement of vacuum bagging materials?