Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Aero Modelling, UAV and Radio Controlled
»
Making a shell for a RC car.
Making a shell for a RC car.
Post Reply
Like
27
Making a shell for a RC car.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Aquaman
Aquaman
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 60
Hi all,
First of all I hope this is the right section to post my query and I can get some expert help and guidance.
I plan to make my own rc car shell as the one on the market for my car is very brittle and snaps at any point of contact.
The requirements of the shell I make are that it has to be strong, doesn't crack/snap upon impacts, must be flexible and long lasting. The reason for these requirements are because the car will be flipping over and landing on it's shell, rolling over multiple times and having impact on the shell from various angles etc..., the car weighs around 15-20kg I believe.
I don't plan to make a mould but rather use the inside of the shell as a mould as I figured it'll save me time, money and it wouldn't look much different from being slightly smaller.
So far I have thought of putting down 1 layer of
Black, 200g Diolen Fabric in a 2/2 Twill weave
for aesthetics. Following that with 1 layer of
Aramid 2/2 Twill Weave 300g Fabric Cloth. This will be followed by 2 or 3 layers of 300g Chopped Strand Mat (fibreglass) then maybe another layer of
200g Diolen Fabric in a 2/2.
What do you guys think of this plan, will it be suitable for my needs? Will it become too thick? Is it possible to bond all those fabrics together without them coming apart easily? Any suggestions and advice will be greatly appreciated.
Also to note I won't be using a vacuum or anything just laying everything down by hand and using a brush to spread any resin.
What else would I require for the job in terms of the type of resin that can be used on all the materials I will be using and also any sort of coating that will go on my mould (inside of rc car shell).
Thanks in advance.
Reply
Like
27
Replies
Dravis
Dravis
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 592,
Visits: 1.9K
Hi there,
What is the shell for your RC car made from?
If it is made from polyester fiberglass you will have some trouble using it as a direct mold.
If the shell is nicely painted on the outside, you should really take the time to make a mold from it, then you can polish the mold and get a nice finish on the CF shell.
How big is the shell? At How many points does it fasten to the chassis? This will determine how many layers you need. You could probably make a very strong impact resistant shell by just using a few layers of Carbon/Kevlar/twaron mixed fibre. Putting glass fibre in will only make it thicker and heavier, not much stronger.
You could consider using EC flexible epoxy resin.. If you do make a mold, then maybe you can sell a few shells to other users of the same model of RC car?
Personally I would use Twaron as outer layer, it has a very nice CF pattern, somewhat enhanced by the different shine of the CF and the Twaron tows, and it is very impact resistant.
If you insist on using the inside of your current shell as a mold, and are not worried about the outside finish on your new shell, then you may get away with just waxing it very thoroughly.
As to tools, do not rely on a brush, when doing larger areas of hand lay up, get a roller, the EC bristle roller is very good, but a b. to clean ...
Good luck
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
Tags
RC car shell Twaron flexible
Edited
13 Years Ago by
Dravis
Reply
Like
28
Aquaman
Aquaman
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 60
Hi,
The stock shell is made from ABS plastic I believe and is brittle.
The shell is of 1/5th scale. After making the shell I would only need to drill 4 small holes for the body posts. Making a mould will just result in more money being used and I really only need to make a reliable shell for 'bashing' as we call it in the rc hobby. Using a few layers of the fabrics you mentioned will make my costs go up quite a bit as those fabrics aren't cheap and I have to take in to consideration the cost of other things such as resin, gloves, gel coat etc... I'll look in to getting a roller also.
Dravis (02/07/2013)
Hi there,
What is the shell for your RC car made from?
If it is made from polyester fiberglass you will have some trouble using it as a direct mold.
If the shell is nicely painted on the outside, you should really take the time to make a mold from it, then you can polish the mold and get a nice finish on the CF shell.
How big is the shell? At How many points does it fasten to the chassis? This will determine how many layers you need. You could probably make a very strong impact resistant shell by just using a few layers of Carbon/Kevlar/twaron mixed fibre. Putting glass fibre in will only make it thicker and heavier, not much stronger.
You could consider using EC flexible epoxy resin.. If you do make a mold, then maybe you can sell a few shells to other users of the same model of RC car?
Personally I would use Twaron as outer layer, it has a very nice CF pattern, somewhat enhanced by the different shine of the CF and the Twaron tows, and it is very impact resistant.
If you insist on using the inside of your current shell as a mold, and are not worried about the outside finish on your new shell, then you may get away with just waxing it very thoroughly.
As to tools, do not rely on a brush, when doing larger areas of hand lay up, get a roller, the EC bristle roller is very good, but a b. to clean ...
Good luck
Edited
13 Years Ago by
Aquaman
Reply
Like
26
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Making a shell for a RC car.
Aquaman
-
13 Years Ago
Hi there, What is the shell for your RC car made from? If it is made from polyester fiberglass you...
Dravis
-
13 Years Ago
Hi, The stock shell is made from ABS plastic I believe and is brittle. The shell is of 1/5th...
Aquaman
-
13 Years Ago
Would appreciate some more of your advice guys.
Aquaman
-
13 Years Ago
Hey man, what you wish to attempt is a huge undertaking, trust me. I made a shell for my bajas, took...
baja_patient
-
13 Years Ago
Hi Aquaman I would say you are using too many layers and with a wet lay you will have a very...
carbonfibreworks
-
13 Years Ago
I did something similar, but with a mould......
matthieutje65
-
13 Years Ago
Post Reply
Like
27
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search