Don't know if anyone can identify this fabric.
Its a carbon twill with what looks like a thread of stainless steel along the warp:



Thanks

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I've been testing Basaltfibre that looks quite similar the last few days,
Are you sure it's carbonfibre?

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Edited 12 Years Ago by matthieutje65
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
Definitely not, basalt isn't used for cosmetic pieces as it oxidises very quickly.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
prairiecustomcomposites
prairiecustomcomposites
Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)
Group: Forum Members
Posts: 26, Visits: 722
Looks exactly like the Silver Reflections Carbon Fiber fabric from Composite Envisions,

http://compositeenvisions.com/raw-fabric-cloth-2/reflections-carbon-fiber-145/silver-reflections-carbon-fiber-fabric-2x2-twill-50-3k-5-9oz-816.html

No idea who weaves the fabric for them, but they carry a bunch of different colours and styles. I have always wanted to try using some - the price tag has kept me from buying it though.
Kevin-Lee
Kevin-Lee
Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)
Group: Forum Members
Posts: 44, Visits: 2.4K
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
From the description, its not carbotanium.
I've sent the photo to Cristex, they should be able to identify it.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search