Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Do you post-cure a part inside the mold, or outside (once demolded) ?
Do you post-cure a part inside the mold, or outside (once demolded) ?
Post Reply
Like
3
Do you post-cure a part inside the mold, or outside (once demolded) ?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jess8bit
Jess8bit
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 133,
Visits: 566
Yeah, again a silly n00b question of mine
And how do you heat it ? simply by placing it in a domestic oven, @60° for some hours ?
thanks guys
!!
Reply
Like
3
Reply
Jess8bit
Jess8bit
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 133,
Visits: 566
ok
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Do you post-cure a part inside the mold, or outside (once demolded) ?
Jess8bit
-
12 Years Ago
Depends on the HDT of the resins in your mould and in the part. Not to mention the release agents...
carboncactus
-
12 Years Ago
Thank you so much for having taken the time to post a detailed explanation, CC ! :) I use EC Uni...
Jess8bit
-
12 Years Ago
The Uni-Mould system is good for 90 Degrees C. Ideally put the mould through a couple of heat cycles...
wozza
-
12 Years Ago
thank you Warren :)
Jess8bit
-
12 Years Ago
..oh and, do you keep the bagging materials while post curing ?
Jess8bit
-
12 Years Ago
Yep leave it in the bag all sealed off with 2 line clamps when you chuck it in the oven. No stink...
Warren (Staff)
-
12 Years Ago
that's great. I was wondering how the bagging materials react when heated.
Jess8bit
-
12 Years Ago
The bag will become a bit brittle but not a problem as that is what it was designed for. Anything...
wozza
-
12 Years Ago
ok :)
Jess8bit
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search