Post Curing IN2 Infusion Resin parts


Author
Message
philiplardner
philiplardner
Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)
Group: Awaiting Activation
Posts: 25, Visits: 65
Hi Matt,

The data sheet for your IN2-Infusion Resin gives the following schedule of times@temperatures for post curing:

24hrs @ room temperature
6hrs @ 40C
6hrs @ 50C
12hrs @ 60C

The Maximum Tg (glass transition?) temperature for the IN2 Infusion Resin is given as 94C - 100C for the slow cure mix. Is this the maximum temperature that this resin can be post cured to or should it be post cured to a lower temp? Ideally I would like to post cure to as high a temperature as possible as the parts are structural and will be subject to intense solar heating at times.

Can you suggest a post curing time@temp schedule beyond the one given above (say to 80 - 100C)? I understand the temperature ramp-up rate can be critical to the finished part's strength.

I am using both 5mm and 10mm thick closed cell PVC foam core material in my laminates - what temperature can this foam board take before it starts to degrade - can it withstand the higher post curing temperatures?

Thanks,

Phil.
Reply
philiplardner
philiplardner
Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)Supreme Being (360 reputation)
Group: Awaiting Activation
Posts: 25, Visits: 65
Thanks Paul.

Phil.