Hi Guys,

I've just experienced my first mold making using Uni-Mould system. My project it to CF copy the "B Pillars" covers of the VW Golf 6 car.
These parts are made of plastic, with a glossy black finish.

So I made a mould this way :
- 4 layers of EC Chemical Release Agent, 30 mn between each
- 1 layer of Model 6 release wax, buffed.
- 1 coat of Tooling GC
- 2 slices of 80g CSM with the Coupling Coat
- 2 slices of 450g CSM with the Tooling Resin.

Demolding was quite straight forward.

Here the problem :
To restore the initial gloss of my part, I used EC Mould Cleaner and lint free wipes to clean the part surface, which was initialy covered by the release agent.
But all I get is a kind of dull, even whitish in some places, surface. Can't get my gloss back. What happened ? 

Thanks for helping, I'm afraid I have damaged the part surface but don't know why...    as if the release agent, or the mold cleaner, had attacked the gloss... Unsure 
Replies
Jess8bit
Jess8bit
Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)
Group: Forum Members
Posts: 133, Visits: 566
Ok, seems the wax is not a popular candidate then BigGrin

Thank you Chris Smile

Jess
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
Jess8bit (18/05/2013)
Ok, seems the wax is not a popular candidate then BigGrin

Thank you Chris Smile

Jess


I use wax all the time for stuff that's not going to cure in the oven. 3 coats, no PVA. I use semi permanents only for prepreg work, they are way too expensive and a waste when not used to their full potential. Don't get me wrong, they work perfectly for this, but its over engineered. If you were using epoxy gelcoat and vac bagging, maybe.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Jess8bit - 12 Years Ago
Jess8bit - 12 Years Ago
carbonfibreworks - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
carbonfibreworks - 12 Years Ago
Jess8bit - 12 Years Ago
carbonfibreworks - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Leon - 12 Years Ago
Jess8bit - 12 Years Ago
carboncactus - 12 Years Ago
Jess8bit - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search