Hi, im new to this forum


Author
Message
carbonrace
carbonrace
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 4, Visits: 23
Hi, im new to the forum and it's a pleasure to discover this factory and its products.
I was the Telco owner, an Italian factory that produced carbon fibre parts for racing cars and motorbikes from 2000. 
I've a good experience in making carbon fibres parts, carbon fibres tubes and fiberglass molds with some different technologies expecially in vacuum bags.
Don't esitate to ask if you need.
  
Regards Alessandro from Italy
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hi, great to have someone new, like you on the forum now!

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




prsw
prsw
Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)
Group: Forum Members
Posts: 112, Visits: 1K
Welcome
great to have you here.


http://motoform.blogspot.se

_GABBER
_GABBER
Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)Supreme Being (483 reputation)
Group: Forum Members
Posts: 41, Visits: 646
ciao benvenuto!!
fgayford
fgayford
Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)Supreme Being (6.5K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
carbonrace (25/04/2013)
Hi, im new to the forum and it's a pleasure to discover this factory and its products.
I was the Telco owner, an Italian factory that produced carbon fibre parts for racing cars and motorbikes from 2000. 
I've a good experience in making carbon fibres parts, carbon fibres tubes and fiberglass molds with some different technologies expecially in vacuum bags.
Don't esitate to ask if you need.
  
Regards Alessandro from Italy
 
Welcome!
Perhaps you could share so pictures of the more interesting projects you have been involved with.
Thanks
Fred
alebassa
alebassa
Supreme Being (596 reputation)Supreme Being (596 reputation)Supreme Being (596 reputation)Supreme Being (596 reputation)Supreme Being (596 reputation)Supreme Being (596 reputation)Supreme Being (596 reputation)Supreme Being (596 reputation)Supreme Being (596 reputation)
Group: Forum Members
Posts: 48, Visits: 171
Ciao e benvenuto! La partecipazione italiana sul forum aumenta a vista d'occhio!

Hi and welcome! Many more italian people on this forum!


Alessandro
carbonrace
carbonrace
Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)Forum Guru (60 reputation)
Group: Forum Members
Posts: 4, Visits: 23
Yes, it's true,
I've a lot of interesting projects to share with you, expecially about motorbikes.
In the next days I will post some photos.

Alessandro




Ortonporton
Ortonporton
Supreme Being (108 reputation)Supreme Being (108 reputation)Supreme Being (108 reputation)Supreme Being (108 reputation)Supreme Being (108 reputation)Supreme Being (108 reputation)Supreme Being (108 reputation)Supreme Being (108 reputation)Supreme Being (108 reputation)
Group: Forum Members
Posts: 8, Visits: 338
Hey Alessandro

I look forward to that, I'm just starting a scooter project where I'm going to make all the bodywork, I'm interested in knowing about bike fairings, and also fixings etc, no one does bikes like the Italians!! 

Cheers gavin
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search