What is the Big Vacuum Pump oil red cap used for ? Plus unknown flasks question.


What is the Big Vacuum Pump oil red cap used for ? Plus unknown flasks question.
Author
Message
Jess8bit
Jess8bit
Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)
Group: Forum Members
Posts: 133, Visits: 566
Hello, I'm ready to operate my big EC vac pump for the first time. I'm a bit confused about what to do with the red cap. What's its role ? I understood I've first to remove the big black fitting cap to poor some pump oil in. But what to do with the small red cap located near the botttom of the handle ?

Plus, I've noticed the pump is shipped with 2 long plastic flasks, with no indcation on them. What's in it ? What's their purpose ? Is that pump oil to poor in ? (does not look like...)

Looks like newbie questions Blush

Thank you for your help,

best regards

Jess.
Smile
sim73
sim73
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Awaiting Activation
Posts: 1, Visits: 5
Yes i also need to know this info i got a unit today,
as i have filled up the small hole with red cap, if i need to drain this i need to know asap!!..

same with the plastic flasks?? no instruction book on the pump?

cheers..
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The red cap is a dedicated oil filling point.  Depending which batch, the cap has OIL written on it in some cases.

The two bottles are full of vacuum pump oil.  They are supplied by the pump manufacturer hence a slight colour difference to the oil we retail seperately, however both oils meet the necessary standards.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Jess8bit
Jess8bit
Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)
Group: Forum Members
Posts: 133, Visits: 566
Thank you very much Warren BigGrin

That means I will pour this *red* hole with the oil coming from hte flasks first, then I will use your retailed oil I also have.

regards,

Jess
Jess8bit
Jess8bit
Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)Supreme Being (841 reputation)
Group: Forum Members
Posts: 133, Visits: 566
For the record Smile

I've filled up the pump with both provided oil flasks. I think it might be a bit much in so far as the level has now reached the Max level  (very top of the sight glass).

But I did not observed any fumes yet.