Having asked the manufacturer, they do not hold any testing data for electrical conductivity or resistance.

The service temperature for cured silicone is -60C to +250C.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ritendramishra
ritendramishra
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 2, Visits: 3
Hi, I am a PhD student in India. I want to know about the electrical properties of the Addition cure Silicone Rubber which you supply. Properties like dielectric strength, resistivity, etc. Also the temperature resistance of this particular grade of silicone.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search