By ritendramishra - 4/27/2013 7:10:57 PM
Hi, I am a PhD student in India. I want to know about the electrical properties of the Addition cure Silicone Rubber which you supply. Properties like dielectric strength, resistivity, etc. Also the temperature resistance of this particular grade of silicone.
|
By Warren (Staff) - 4/29/2013 9:38:00 AM
Having asked the manufacturer, they do not hold any testing data for electrical conductivity or resistance.
The service temperature for cured silicone is -60C to +250C.
|
|