To me that looks like a shaddow marking of the backing that would originally have been on the UD sheet before manufacture. Many UD type sheets have a fine supporting net of thread either within the UD or on the back of it. The ones ive seen look just like that criss cross pattern.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|