Hey ahhh, why these parts getting so soft in the sun?

 

How can I fix this? I do resin infusion, is it time to get a parts oven and switch to a higher temp tooling gel?



If Brute Force Isn''''t working your not using enough...
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I've once seen a picture on the internet of a guy curing his parts in the sun, this is how he did it.

You take a carboard box, put you part in it, put a black trashbag arond the box, make some small holes in the bag with a knife, put it outside on a hot summer day Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Carbon Tuner - 13 Years Ago
NikCFC - 13 Years Ago
             whats post cure?
Carbon Tuner - 13 Years Ago
SebRS - 13 Years Ago
NikCFC - 13 Years Ago
Bruce - 13 Years Ago
Matt (Staff) - 13 Years Ago
Bruce - 13 Years Ago
ebf2k - 12 Years Ago
Carbon Tuner - 13 Years Ago
Joe - 13 Years Ago
Warren - 13 Years Ago
twissta - 13 Years Ago
Warren - 13 Years Ago
Carbon Tuner - 13 Years Ago
Warren - 13 Years Ago
Ortonporton - 12 Years Ago
TomDesign - 12 Years Ago
NikCFC - 12 Years Ago
matthieutje65 - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search