Carbon Fibre Cloth Fabric
»
Coloured Carbon extra reinforcement?
Coloured Carbon extra reinforcement?
Post Reply
Like
6
Coloured Carbon extra reinforcement?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
k9gti
k9gti
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 18
Hi,
What sort of layering would you suggest for using coloured carbon cloth to make car body panels? I am looking at making a carbon engine lid (resin infused process) for my '73 Beetle, for road use. Since the coloured cloth is a carbon/polyester blend and so has less strength that plain carbon I assume it needs a secondary layer behind it? I was thinking of 1x 210g Colour cloth, 1x regular 200g carbon, a 2mm Soric core layer, and then another plain carbon inner 200g layer for the inner, plus extra strengthening around the outer edges (seal, hinge & latch positions) and numberplate light mounting area. Would this be strong enough? I think this would make it about 2.75mm thick. Would this be a good strength for a road car? Or would you recommend a 3mm core or more carbon layers?
Thanks for your guidance! :-)
Nigel
Reply
Like
6
Replies
Warren (Staff)
Warren (Staff)
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
For really lightweight panels, a single layer of carbon either side of 3mm soric is about as light as you can go.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
6
k9gti
k9gti
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 18
Thanks - I know that is the ideal for regular carbon, but what do you suggest for using the coloured carbon which isn't as strong? Does it need an extra normal carbon layer before the Soric? As I said, it's a road car so ultimate lightness isn't the highest priority - it needs to last as well.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Coloured Carbon extra reinforcement?
k9gti
-
13 Years Ago
For really lightweight panels, a single layer of carbon either side of 3mm soric is about as light...
Warren (Staff)
-
13 Years Ago
Thanks - I know that is the ideal for regular carbon, but what do you suggest for using the coloured...
k9gti
-
13 Years Ago
Hi in my experience the issue is not one of strength. In the application you are describing there...
wozza
-
13 Years Ago
Thank you Warren - that was very helpful :)
k9gti
-
13 Years Ago
ive found that the coloured carbon allows slightly more twist in the part. for christmas i came up...
ajb100
-
13 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search