help cracks in mould


Author
Message
Daz
Daz
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 93, Visits: 651
Hi Warren,

This is the mould i have made of my roof which i intend to cut off



I havnt made a carbon part as of yet

I hope it does release better than the mould on the car,

Ps

I need some rs 500 carbon bonnet vents Wink
Edited 13 Years Ago by Daz
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Daz (05/02/2012)
Thanks for the replys ,

Yes good news Joe

I think its going to be a goer

Have filled the cracks with the new black gel coat ,,


You now owe me a track lap in your carbon fiber Dolomite Tongue

Joking... but happy it turned out good.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
Daz
Daz
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 93, Visits: 651
Joe (05/02/2012)
Daz (05/02/2012)
Thanks for the replys ,

Yes good news Joe

I think its going to be a goer

Have filled the cracks with the new black gel coat ,,


You now owe me a track lap in your carbon fiber Dolomite Tongue

Joking... but happy it turned out good.


loL
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
I believe your cracks are the result of having your gelcoat too thick, any bending of the mold will crack thick gelcoat.

The best way to fix it is to V out the whole crack and then mix up some of the same gelcoat you used and build it up layer by layer. If you get gravity

on your side fill the crack just barely and put a tightly stretched piece of clear packaging tape down over it. It will flatten things down quite well. Once cured you will have to carefully bd sand the repair down flat and polish. I use 2 or 3 inch pieces of paint sticks.

Another thought. You will wax the mold on your next part anyway so wax will seal the crack. Your part will have a slight crown which is easy to sand down.

Fred
CarbonMike
CarbonMike
Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)Supreme Being (221 reputation)
Group: Forum Members
Posts: 31, Visits: 45
fgayford (11/12/2012)
I believe your cracks are the result of having your gelcoat too thick, any bending of the mold will crack thick gelcoat.

The best way to fix it is to V out the whole crack and then mix up some of the same gelcoat you used and build it up layer by layer. If you get gravity

on your side fill the crack just barely and put a tightly stretched piece of clear packaging tape down over it. It will flatten things down quite well. Once cured you will have to carefully bd sand the repair down flat and polish. I use 2 or 3 inch pieces of paint sticks.

Another thought. You will wax the mold on your next part anyway so wax will seal the crack. Your part will have a slight crown which is easy to sand down.

Fred


As already here really. Although its also very easy to repair really minor cracks in moulds using super glue. The same why you can secretly repair repair carbon with basically.