Hi guys

I'm Rob, currently in the UK. I'm here to talk carbon fibre and its limitations, and get guidance on a very ambitious project that I'm looking at doing!

So - a couple of generalised questions first off:

What are the pressure limitations of carbon fibre? Any particular sort of method to moulding that will give a better pressure rating?
What kind of extreme angles can I get out of carbon fibre?

Cheers!

Rob
Reply
emisnug
emisnug
Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)Junior Member (15 reputation)
Group: Forum Members
Posts: 3, Visits: 34
Well, I've got a carbon fibre bottle that holds 4500psi Smile I have no idea as to the wall thinkness of the tank though.

As far as material testing - first I need to make it. I've got an idea of having a mould, but I wouldn't know how to join the two halves together, and seeing as it is a pretty complicated, air-holding shape - the joins need to be spectaculararly good. Any ideas anyone?