Quesiton To All! : Flat Panel Mould


Author
Message
Dave
Dave
Supreme Being (660 reputation)Supreme Being (660 reputation)Supreme Being (660 reputation)Supreme Being (660 reputation)Supreme Being (660 reputation)Supreme Being (660 reputation)Supreme Being (660 reputation)Supreme Being (660 reputation)Supreme Being (660 reputation)
Group: Forum Members
Posts: 48, Visits: 253
Hey there fellow Composite Nuts!

I have been making various parts however now i am needing to create a perfect flat panel with a perfect gloss finish... currently looking at various panels/sheets that will be strong enough not to warp or ripple at all and keep scratch free so that either a large fiber glass mold could be made from or infuse off directly.

What economical CHEAP ways do you guys go about obtaining this surface finish?

I have been looking at acrylic panels (although getting a large one isn't very cheap) and whilst writing this post i think later i will have a look at large mirrors.)

Cheers,
Dave.
Edited 14 Years Ago by Dave
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)Supreme Being (10K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I did an infusion once on a mirror and everything went perfect after 6 coats of  Meguiars Hi-Temp Mouldrelease.
About the cleaning of the glass, you could use some acetone in think to remove the sticky resin pattern on the glass

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dave - 14 Years Ago
Anarky - 14 Years Ago
r0bsk1 - 14 Years Ago
pk_090 - 14 Years Ago
CarbonMike - 14 Years Ago
ajb100 - 14 Years Ago
Matt (Staff) - 14 Years Ago
tauruck - 13 Years Ago
Dave - 14 Years Ago
carbonfibreworks - 13 Years Ago
matthieutje65 - 13 Years Ago
Dennis G - 14 Years Ago
Warren - 14 Years Ago
carboncactus - 13 Years Ago
fgayford - 13 Years Ago
Kevin-Lee - 13 Years Ago
pk_090 - 13 Years Ago
Leew - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search