Hi,

I want to make my Clio´s bonnet, but i´ve got question:

Because it´s a part that will be exposed to the sun, do i have to use a resin resistant to the UV?

If i use a simple polyester resin, will it be "yellowed" with time?
Replies
brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
sweep it out, then blow it out,and then wet everything with a hose and water. if the air temps are down you can have humidity issues. make sure you
get cool temperature activators. and let the coats get dry...almost before the next coat. if you touch the clear and when you pull away it leave strings of clear like spider's silk, then it is ready for next coat. dont lay the part on cardboard,as that is a major dust magnet.
CF probably has static electrcity issues...if it does before spraying mix some water and alcohol in a spray bottle and lightly spray the part and that will
discharge the static electricity. then wipe it clean Smile

scott


CarbonFiberCreations



fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Hi Scott

Water and alcohol is a good static charge eliminator? What ratio? I was thinking of getting a anti static gun, real expensive.

I like this method better if it works. Can you explain how you found this out and how you use it in your auto refinishing.

Thanks

red
brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
woot! PPG had a product to wipe down raw plastic bumpers before sealing and refinishing, it was alcohol and water. it was a low VOC product and
it did not eat into the Mazda factory primer on the new bumper covers from Mazda.
not sure of ratio, maybe try 50/50 and see how it does?i suppose more alcohol would be ok or 100% as well, it will evap fast.
i could feel the static field diminish as i sprayed it. wierd !
i think glass cleaner will do the same as well. painting auto plastic bumpers has all kind of problems LOL.
seems to me we get the same issues with new FG truck parts as well, all sanded and clean and static. i suppose one could also ground the underside of the part and the floor as well???



scott


CarbonFiberCreations



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search