i got my filleting wax today!! thanks guys at Easy Composites !!


CarbonFiberCreations



wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Right no excuses now get that boot spoiler on the go!!!!Smile
Not sure what the weather is like where you are but here in the cold U.K I find sticking the wax in a plastic bag and putting in warm water for 15 minutes makes it much more "workable".

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search