|
Group: Forum Members
Posts: 3,
Visits: 8
|
Many thanks for the advice. I was really hoping to laminate with it but I might have to settle for a coating. There have ben similar issues with some of these tank sealers but there is one on the market that everybody seems to swear by. I'll have to research it further and get back to you. If you haven't glued the 2 halves of your tank together yet, have you thought about having a flexible bladder made for it out of Viton or similar. This is what I was going to do but for the number of tanks I want to make of one shape this would be cost restricitve. However, if you've gone to the trouble of making a carbon fibre tank you might be happy with the cost. I can supply details of a good manufacturer if you want it.
|