Carbon Overdose by CFC


Author
Message
NikCFC
NikCFC
Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)
Group: Forum Members
Posts: 61, Visits: 871
My latest project V-Carbon GSXR 1000 K6 made via Vac.Infusion - GSXR750K6 & CBR600RR












Edited 13 Years Ago by NikCFC
TomDesign
TomDesign
Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)Supreme Being (5.6K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
great!

where to get that patter carbon cloth or bigger waves?
prsw
prsw
Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)
Group: Forum Members
Posts: 112, Visits: 1K
That looks great, do you use stabilized fabric? (C285T4s)


http://motoform.blogspot.se

Edited 13 Years Ago by prsw
NikCFC
NikCFC
Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)
Group: Forum Members
Posts: 61, Visits: 871
TomDesign (21/02/2013)
great!

where to get that patter carbon cloth or bigger waves?


I think there is available in the market an already made V pattern cloth, but in the photos you see I made the V pattern using two pieces of cloth.
NikCFC
NikCFC
Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)
Group: Forum Members
Posts: 61, Visits: 871
prsw (24/02/2013)
That looks great, do you use stabilized fabric? (C285T4s)


Nope it was ordinary carbon 4x4 twill fabric
prsw
prsw
Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)
Group: Forum Members
Posts: 112, Visits: 1K
NikCFC (25/02/2013)
prsw (24/02/2013)
That looks great, do you use stabilized fabric? (C285T4s)


Nope it was ordinary carbon 4x4 twill fabric


Ok, then I am even more impressed.
How did you stop the fibres from falling apart at the cut?
tackspray, hairspray, or just mega skills? :-)


http://motoform.blogspot.se

NikCFC
NikCFC
Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)Supreme Being (855 reputation)
Group: Forum Members
Posts: 61, Visits: 871
Thanks! Tackspray and being really really carefull!!!
Edited 13 Years Ago by NikCFC
BoostSamurai
BoostSamurai
Supreme Being (486 reputation)Supreme Being (486 reputation)Supreme Being (486 reputation)Supreme Being (486 reputation)Supreme Being (486 reputation)Supreme Being (486 reputation)Supreme Being (486 reputation)Supreme Being (486 reputation)Supreme Being (486 reputation)
Group: Forum Members
Posts: 34, Visits: 413
Fantastic work that just makes ones mouth water Smile

JZX World Forums
VVS
VVS
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Moderators
Posts: 226, Visits: 334
Beautiful work, bikes look the bollox!




I'm in the middle of making fairing moulds and will be trying my first infusion this week.

What thickness of carbon have you found best for your fairings, I'm looking for lightness without suffering wind vibration,

I was thinking 3 layers of 200grm cloth, with maybe a piece of Kevlar on the mounts.

have you found a happy medium with your lay-up.




Chris.
Jacopo Carbonio
Jacopo Carbonio
Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)Supreme Being (589 reputation)
Group: Forum Members
Posts: 43, Visits: 109
Wow! Incredible result! Good looking carbon fiber 4x4 Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search