Hey guys let see if you can help me, I am trying to skinned a product, with carbon firbre, I was told to add catalyst to epoxy. Do this really needed? what is the sense of adding catalyst to epoxy if the epoxy is a laminar glue
Replies
brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
it will not work without the catalyst. and it must be mixed thoroughly as well or it will never fully cure as well.


CarbonFiberCreations



dei
dei
Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)Supreme Being (125 reputation)
Group: Forum Members
Posts: 15, Visits: 130
Thank you very much for your quick responds...
According to the seller, he told me that the epoxy contain 3 component, that there is no need for catalyst. I am new to firbre carbon and epoxy, I would like to be sure of what I am doing before I made a mistake

brasco (16/02/2013)
it will not work without the catalyst. and it must be mixed thoroughly as well or it will never fully cure as well.

fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
brasco (16/02/2013)
it will not work without the catalyst. and it must be mixed thoroughly as well or it will never fully cure as well.



I go so far in mixing that I always double cup just to make sure its thoroughly mixed. By that I mean, I mix thoroughly in one cup and then pour the mix into another clean cup and continue mixing with a new stick. Why you might ask? I have got burn't  with polyester gelcoat not being mixed thoroughly. The result is what I call cancer (crocodile skin, wrinkles etc)
Epoxy is so expensive I feel it worth the added insurance of a complete mix.
Hope this helps.
Fred
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
dei - 12 Years Ago
brasco - 12 Years Ago
dei - 12 Years Ago
fgayford - 12 Years Ago
Shaneer22 - 12 Years Ago
Shaneer22 - 12 Years Ago
dei - 12 Years Ago
brasco - 12 Years Ago
brasco - 12 Years Ago
Warren - 12 Years Ago
dei - 12 Years Ago
brasco - 12 Years Ago
Warren (Staff) - 12 Years Ago
wozza - 12 Years Ago
dei - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search