Killed my Dremel


Author
Message
NikCFC
NikCFC
Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)Supreme Being (839 reputation)
Group: Forum Members
Posts: 61, Visits: 871
mmm probably you should remove the silicone from the gaps ASAP because the motor of the vac cleaner needs to breath....you can you a piece of cloth instead, which will block the dust but not the air
pk_090
pk_090
Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)Supreme Being (623 reputation)
Group: Forum Members
Posts: 47, Visits: 169
Ive rigged up a separate inlet pipe and fan to cool the motor out that sucks in air from a safe area away from dust, the silicone is there purely to stop the dust after its been sucked up disappearing though panel gaps before it gets to the collection point. 
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I know this is a very old topic, but just thought I'd post seeing as I was reading through...



For my dremel, I cut up a dust mask and secured the pieces over the vents on the tool. I replace the pieces of mask when they start getting a bit clogged up. Works very well, no issue with the tool overheating and no issues with dust. Prior to doing this, I went through 3 cheap rotary tools, and took the occasional electric shock to the hand during operation...
fgayford
fgayford
Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)Supreme Being (6.4K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
fgayford (25/01/2013)
Probably a good idea to blow out your dremel with compressed air every once in a while.

Fred


Well here is an update. My Dremel is now toast. Carbon dust is highly conductive and shorts things out. I bought a new Dremel  and the long flexible shaft and everything seems fine now.
Fred

morepower
morepower
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
I swapped the fuse for a 1 amp fuse.. Too low to fry the dremel but high enough to let it work.. I was popping them and fried my old dremels but oddly since I swapped to 1amp I have been lucky and not fried it yet.. although the speed control does not work.. lol... I used to wrap the body with some breather cloth.. it worked OK.. 

Oh by the way... The original fuse was 3 amp... I wanted it to blow the fuse before it could do anything to the motor.... I am not increasing the rating of the fuse.. NOT A GOOD IDEA...
Edited 12 Years Ago by morepower
wildcard
wildcard
Supreme Being (466 reputation)Supreme Being (466 reputation)Supreme Being (466 reputation)Supreme Being (466 reputation)Supreme Being (466 reputation)Supreme Being (466 reputation)Supreme Being (466 reputation)Supreme Being (466 reputation)Supreme Being (466 reputation)
Group: Forum Members
Posts: 40, Visits: 406
Subscribing... I burnt mine up yesterday. I let it cool for the night. Hopefully it will start again today. If not I'll be trying some of the tricks in this thread. 