can someone help with this thing for vacuuming?
can someone help with this thing for vacuuming?
Post Reply
Like
3
can someone help with this thing for vacuuming?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
guys just got big order from easycomposites. can someone help how i have to use this connector ? so i can use my part for only vacuuming .
how everything work with this item. and how to connect to vacuuming pump. sorry that way i do first time and any help welcome. so i can connect and start vaccum bag. as i dont think im missing anything here.
Reply
Like
3
Reply
TomDesign
TomDesign
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
i got those 2 pieces in link.
but i saw video i dont have piece and not see here that bolt on top of mine piece?and that go on a pipe from vacuming pump. someone help to link from easycomposites so i can order and my vacuuming bag can work perfect.
Thanxs
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
can someone help with this thing for vacuuming?
TomDesign
-
12 Years Ago
You need brass non return 1/4" plug. Quick release 1/4" bps. Bsp hose tail fitting use ptfe tape to...
Shaneer22
-
12 Years Ago
can you please link from easycomposites so i can order. Thanxs
TomDesign
-
12 Years Ago
You could connect it to the pipe with valve and a pipe fitting the parts below...
Bruce
-
12 Years Ago
i got those 2 pieces in link. but i saw video i dont have piece and not see here that bolt on top...
TomDesign
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search