I'm new to this whole composites thing and have started pulling parts from my first mould. It was made using the EC gel coat and I sanded down to 1500 grit. As the finish isn't important I didn't go down the polishing route on the plug or the flanges.

I've created a few parts now.. I used the easylease chemical release agent 5 applications. . During layup and while curing under vacuum I get a thin film of epoxy curing on the flanges. I clean what I can using malt vinegar during layout but there is still some spread during vacuum. When releasing the part this dried epoxy  remains on the mould flanges and I have to remove it manually. It hasn't adhered completely to the mould in most places. But in a few no amount of co-ersion with a wooden part or steel blade will get it off. As a result I'm scratching the mould surface while cleaning this off and i'm reducing the life of my mould a lot. 

Any ideas or suggestions to prevent this?

Thanks in advance!
Edited 12 Years Ago by Philimon
Reply
neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
silicone sealer on the parting flanges is great, you can also wipe off excess if it enters on to the mould surface quite easily, would sort your problem out