I've been making flange out of chopped strand matt for years but I must say sign board is cheaper and  nothing bonds to polypropylene making your own costs more and you can't cut with blade,so I recommend sign board.  
Shaneer22
Shaneer22
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 156, Visits: 14K
I've been making flange out of chopped strand matt for years but I must say sign board is cheaper and  nothing bonds to polypropylene making your own costs more and you can't cut with blade,so I recommend sign board.  
Philimon
Philimon
Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)
Group: Forum Members
Posts: 14, Visits: 68
Oh what I'd give for a compressor, spray gun and somewhere to use it...

I do all my compositing in the lounge in front of my TV.

Yes, I did just made that word up.
brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
glad i could help Smile trying to find useful info and share it here. and having the info plus being able to see someone
do it--is priceless!
long live the black arts !!


CarbonFiberCreations



jonnyl888
jonnyl888
Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)Forum Member (38 reputation)
Group: Forum Members
Posts: 6, Visits: 16
Thanks, that really helped. Never really though about using strands of woven glass fibre for edges and ripping up CSM. Looks like I'll save some money by not buying the putty. BigGrin
brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
i think this guy is an experienced mold maker. looks good and clean and no repeating steps.
well done


CarbonFiberCreations



brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
part two




CarbonFiberCreations



brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
GREAT video of how to for a flanged mold .
i first thought the use of fiberglass to make his edging material was not a good idea, but actually it was brill.
i think we all should be sure to keep some FG and Polyester around for this sort of use.

[YouTube]http://www.youtube.com/watch?feature=endscreen&NR=1&v=gzng9HeGNPE[/YouTube]


CarbonFiberCreations



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search