Hi

Would easy lease work on a mould that has been sealed with a sealer?

/Petter


http://motoform.blogspot.se

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hi Petter,

If the sealer has left you with a properly sealed, non pourous smooth surface ready to mould off, then our Easy-LeaseChemical Release Agent will have no problems being used as a release agent. You would need to apply several coats in accordance with the instructions.


The reason sealers are used is to give the plug/pattern a suitable surface to mould from.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
prsw
prsw
Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)Supreme Being (1.6K reputation)
Group: Forum Members
Posts: 112, Visits: 1K
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search