Leon
Leon
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 59,
Visits: 606
Hii guys,
I need your advice for combination of composites material that can provide a several purpose below on 1-2mm thickness:
Light (30-50% than steel)
Stiff (no tik tok)
Cheap (as cheap as good)
This structure criteria is for electric car exterior body such as Hood, Doors, Trunks, fender, spoiler. this car will passion to reducing weight and increasing performance. And segmented for midle-low customer budget, hard to say that the carbon fiber is not an option. Is there any body have a advice? example: biaxial fiber glass+lantorsoric+biaxial+vinyl ester.
Your help are necessary.
Leon
Reply
Like
3
Reply
Jack.Strong
Jack.Strong
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 52,
Visits: 549
Honeycomb panels. Company i worked for "TRB lightweight structures" did work with an electric car, forgotten its name.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
[Ask] Light, Stiff and Cheap
Leon
-
12 Years Ago
Isn't sheetmetal the most suitable for this application, seeing your demands?
matthieutje65
-
12 Years Ago
[quote][b]matthieutje65 (24/01/2013)[/b][hr]Isn't sheetmetal the most suitable for this application,...
Leon
-
12 Years Ago
Honeycomb panels. Company i worked for "TRB lightweight structures" did work with an electric car,...
Jack.Strong
-
12 Years Ago
use plastics. no corrosion-- wont dent easily-- can be made in the color you need-- you will need...
brasco
-
12 Years Ago
What Brasco says brings me on an idea... If you have the budget and time to make some mould and need...
matthieutje65
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search