Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Resins, Gelcoats and Pigments
»
Surface preparations for best adhesive results
Surface preparations for best adhesive results
Post Reply
Like
4
Surface preparations for best adhesive results
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
funkstar
funkstar
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 7
Hello
As the topic says I am wondering about the do;s and dont;s when it comes to fixing both carbon - carbon and alu - carbon stuff togehter. The acutal project I am having will include gluing angular carbonfibre sections to a foam sandwich. As the surfaces are clear I would instinctively use some abrasive to make the epoxy (ET500) grips better. good or bad? what are the thumb rules?
also wondering about how to apply the glue when making a aluminium honeycomb sheet. do I roll it out like paint and then stick the aluminium honeycomb on to the plate or is there another/better method?
Thanks
Per
Reply
Like
4
Reply
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Hi Funkstar,
We always recommend giving the surface a good key before using any adhesives or bonding anything to it. Generally any medium to coarse papers are fine. However remember afterwards to ensure the surface is clean and free of sanding dust before you attempt any Bonding.
For bonding aluminium honeycomb sheet we have our
ET538 Honeycomb Bonding Epoxy Adhesive
which you would ideally spread out in an even layer using a credit card sized piece of plastic as a spreader.
One tip with honeycombs is when you place the honeycomb in the glue layer, give it a slight wiggle in place so that the glue seats nicely around the aluminium cell edges. This will give a slight miniscus of glue on the cell edge ensuring a better bond than if the honeycomb was just sat ontop of the glue.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Surface preparations for best adhesive results
funkstar
-
12 Years Ago
Hi Funkstar, We always recommend giving the surface a good key before using any adhesives or...
Warren (Staff)
-
12 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search