wanted to share Mansory video of making carbon fiber stuff


Author
Message
TomDesign
TomDesign
Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)Supreme Being (3.3K reputation)
Group: Forum Members
Posts: 454, Visits: 2.5K
http://vimeo.com/44927630

i hope guys you enjoy like i did watching this video. As what i saw so far their quality on top.
Reply
_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
Tom, Pagani use T4 twill, I know 285 gr/m2 and 450 gr/m2. It's very expensive, 285 costs about 50€/ M2