Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Hand Layup
»
Epoxy Resin or Polyester Resin
Epoxy Resin or Polyester Resin
Post Reply
Like
3
Epoxy Resin or Polyester Resin
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
RRE
RRE
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 12,
Visits: 33
Which is the best to use? As I understand it, if I am painting the parts its ok to use epoxy, but if I plan to leave it unfinished, then its best to use polyester. Is this correct? Also, is it recommended to use a gel coat first then the resin or just go straight resin? I want my parts to be as lite as possible. I am trying to make my parts around .040 - .050 thick. I tried making my first panel just as a test run and it came out ok, but when I go to make my parts for real I want to make sure they are the best they can be. Does anyone have any suggestions or tips?
I attached a pic of what I am trying to replicate. You can see what is carbon here. Bascially all the cosmetic panels and hood are what I want to make.
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
I have no idea why polyester should be better to leave unfinished?
The finish will 99% be the same between epoxy and polyester... the big difference is that epoxy is supposed to be stronger... this is what your looking for I guess
But, polyester is cheaper than epoxy...
I wouldn't use a gelcoat and just go for the epoxy, since your looking for light parts...gelcoat will add some weight.
If you want to paint your parts sand them a bit (or use peelply in your lay-up) then use a plastic primer and add a clearcoat or colorcoat.
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
RRE
RRE
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 12,
Visits: 33
I am being told polyester has better UV protection than epoxy.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search