definitely do NOT use any buffing products like polishes as they will REMOVE all the easylease due to the fine cutting agents in them.
In effect youre just looking to buff the surface lightly with a lint-free cloth to remove any excess or variation in thickness of the easylease and to even the gloss finish. you wont need to use much force at all really.
Glass when compared to a typical hand laid mould has an almost PERFECT surface finish which is also very hard so any variations in a release agent will show up dead easy.
|