			            How hot is the exhaust getting? 
  You may need to post cure both your resin and the lacquer to maximise their heat resistance.  However if the exhaust is conducting a lot of heat, you may still be overheating the resin.                 
			            
  				
			            Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant                     
                     
                                            
                         
                    
                  
             |