have come accross some cloth called 'basalt'

''Basalt fibre is in alot of ways a better alternative to fiberglass, made from basalt, a hard, dense, volcanic rock. It provides high temperature performance and superior strength''

 

anyone heard of this or is this called something else in europe?

or is this spiel a load of cr@p
Replies
prairiecustomcomposites
prairiecustomcomposites
Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)Supreme Being (184 reputation)
Group: Forum Members
Posts: 26, Visits: 722
I haven't used basalt fibers in composites myself, but I know they are used in higher performance skis and snowboards to add stiffness (just like carbon is). As far as I understand, basalt's performance is in between S-glass fiberglass, and carbon fiber; it is stronger and lighter than the fiber glass but weaker and heavier than carbon fiber, and the pricing is usually in between the two as well.

If I recall correctly, basalt also has a higher compressive strength than carbon fiber. I thought I remember reading that somewhere, but maybe someone on this forum can confirm that. It would also be a good material for getting the "carbon fiber look", without the huge expense.

-Mike-
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
http://www.basaltex.com/en/products.aspx

you can find more information on this website... It's a company located in belgium, but with a website written in english

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
there is black FG in twill weave if you need the look and not the price and performance.
just sayin Smile


CarbonFiberCreations



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search