Group: Forum Members
Posts: 36,
Visits: 664
|
I'm trying to reboot this thread as a sort of build log and I'll try to continue keeping it updated regularly to help me keep my focus. Today is a repair day. I had a part of the edge of the flange a bit too tight to fit but that flange was darn strong. As I pressed in, a weaker part of the frame gave way and I had a full transverse crack run all the way through (top and bottom.) It was still holding its shape and everything was still positioned okay, but I wanted to try to get it fixed. I'm not doing all this work to cut that corner!
I filled the crack with as much epoxy as I could press down into it without fully breaking the frame into two halves. I then skimmed over with more epoxy on all 4 sides. I'm hoping that will give it the structure I need but if it doesn't I'll grind down and create a wire lath to bridge across the break then redo the epoxy over top of it.
I hate setbacks. Silver lining: all this patchwork is improving my skills, but I wish I could get them some other way.
|