Hy guys. 

I have a bit of a problem. I was covering part with heavy carbon sleeve in 2 layers. Method was wet layup with vacuum baging. I calculated resin, covered everything with it and placed in vacuum. After curing carbon is in place and is fairly strong but it it seems that it got just semi saturated.

Is it possible to cover and dab resin into fabric or something else or piece is ready for recycle bin?

Main issue is that it is in 2 layers so I would like to be sure that under layer is saturated as well as upper one
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search