Hi,

Could anyone inform me about inexpensive materials to seal wood that will be used for both silicione mold making and later to cast epoxy over? Would beeswax do the trick or do I need something else?
Rosta Spicl
Rosta Spicl
Supreme Being (804 reputation)Supreme Being (804 reputation)Supreme Being (804 reputation)Supreme Being (804 reputation)Supreme Being (804 reputation)Supreme Being (804 reputation)Supreme Being (804 reputation)Supreme Being (804 reputation)Supreme Being (804 reputation)
Group: Forum Members
Posts: 54, Visits: 250
Low viskosity laminating epoxy resin. Or something more sofisticated and expensive just like Dunapox, Marbocote sealers.