Better releasing peel ply?


Author
Message
The Mould Destroyer
The Mould Destroyer
Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)Supreme Being (213 reputation)
Group: Forum Members
Posts: 21, Visits: 332
I'm dying with my peel ply, every time its a battle 
Are there any advancement in this area? any better releasing peel ply?

Alternatively - any other way to create a good bonding surface?
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Cut it into strips on the edges to help ripping it off.  I am not aware of any "easier" peel ply other than silicone coated ones which with experience are still not easy to remove and cause the secondary bonding issues Hanaldo mentions. 

As peel ply gets saturated with resin, it is not reusable.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search