Group: Forum Members
Posts: 4,
Visits: 33
|
I have a carbon fiber race canoe that was originally constructed using vinyl ester. The hull is being patched using epoxy and carbon and then refinished with and epoxy/ graphite mixture. I have seen information the mentions a wash/ surface prep is required prior to using the epoxy. I haven't been able to locate any information on what is required for the prep. THank you in advance for any and all assistance.
Gary
|