I have some large car moulds
At strateg points it has threaded bosses moulded into the main mould that once your main part is laminated you screw a bolt into the boss and it helps "pop" your item from the mould
Anyone know a supplier in the uk ???
I need too make a couple more moulds an would be easier too have some off these in the mould too help with part removal
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Not a BigHead? Have you got a picture?
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Hanaldo - 12/28/2020 9:54:11 PM
Not a BigHead? Have you got a picture?

No not a bighead but essentially the same just bigger.
Seen on a few other moulds through the years so know its not a one off
"T" bar that screws into the bush when you pop a part out is a very square " acme" style thread about 16/18mm o/d