			            Is it a high temperature wax? And if it is, can it actually handle the temperature you are curing at? Lots of 'high temperature' release waxes are really only designed to handle higher exotherm temperatures, which aren't really that high - often only 80-100° C. I think the highest I have come across is 115°. 
 
 
 |