Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Once fully cured, the resin cannot generally be softened with heat. If it is a fresh pour and has not had a post cure, heat will often soften it slightly which in thinner sections can cause deformation and distortion. A post cure will stop that from happening.
In terms of bending the wings, it may be possible on a fresh cast but you would need to experiment to see if you can find a balance that works.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|