Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Yeh I sort of agree with Lester, I've tried all sorts of dust extraction methods (not specifically any of the ones mentioned in this thread though, so potentially these are better) and just found that at best you capture/extract maybe 50% of the dust. Obviously that is better than none at all, but not a whole heap in practise. You still end up with dust everywhere in the workshop and covered in it yourself. I wouldn't say it isn't worth trying, but my comment would be that my efforts have been pretty much in vain as of yet.
|