Epoxy Coating Resin can be sprayed?


Author
Message
pedcrist
pedcrist
Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)Supreme Being (377 reputation)
Group: Forum Members
Posts: 42, Visits: 350
Hi,

Can your Epoxy Coating Resin be sprayed with a spray gun?

If affirmative, what nozzle should i use? 2,5mm?

Pedro
Reply
Dennis G
Dennis G
Supreme Being (346 reputation)Supreme Being (346 reputation)Supreme Being (346 reputation)Supreme Being (346 reputation)Supreme Being (346 reputation)Supreme Being (346 reputation)Supreme Being (346 reputation)Supreme Being (346 reputation)Supreme Being (346 reputation)
Group: Forum Members
Posts: 34, Visits: 837
fgayford....Do you have any tips for spraying the 2K clear? What do you use for release, easylease? or wax and pva? How many coats? How heavy? Any tips would be appreciated. And would the application change depending on the release agent/s used? I will be using easylease.

Thanks,  Dennis