the carbon with soric is not bad, The problem with glueing is that any axial and angled force can breake the bond du to deformation in the bonded area. Definetly MMA because it allows a bit of movement, Epoxy will just snap once the max force is exceeeded As said in another post, if epoxy goes it goes with a bang, there are usally no warnings or signs of stress before that happans.
After all that all is subject tio testing, with a soric SF core, using rivets or bolts should not be a problem but need penny washers with a nylon between fibre and metal or backplate
|