Also, just for future knowledge - don't use acetone to clean moulds, it will damage the surface. Its too late now and it will probably be fine, so I wouldn't worry too much about it; but in future it is a good idea to use a proper mould cleaner or if you can't get that then a wax and grease remover will work too.
|
|
|
Hanaldo
|
|
Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
+x+x+x+xHello guys, newbie here  Recently i created my first negative mould and used up most of the epoxy gel coat on that. so im working on this very small negative mould as big as my hand. i just finished polishing the actual part's top surface that i should be spreading my gel coat on. The thing is i want to use the remaining epoxy gel coat on my next item and i dont have enough at the moment for the both parts. So is there an alternative to gelcoat that i can make with epoxy resin? I have some fumed silica, i was thinking may be i can use it to thicken the epoxy and use it instead of gel coat. has anybody tried it? my approach on my first mould was 2 coats of gel coat on top of the part. leave it to cure but when its still tacky i applied fiberglass with epoxy and then vacuum the whole thing. as a release agent i bought Easy-Lease Chemical Release Agent, PVA release agent, number 8 release wax and MANN ease release 200 spray i guess i have enough release agents but im not really sure which one works better. i read PVA is almost guaranteed so i used it in my first mould and i guess i brushed it too thick so it gave me abit of a problem during demoulding. Can i just use MANN spray as a release agent as it is very easy to use, is it reliable? Thanks Yes it does work, I just add a thix powder called Cabosil to get a good consistency. It takes a while to blend in well and you need to be sure it's not too thin as epoxy resins seem to separate/fisheye on release agents pretty easily. im thinking abit more thinner than a peanut butter consistency just enough to hold on vertical walls. when cured but still tacky i will lay some fiberglass and i hope its going to work. thank you for the response. have you tried MANN spray or Easy-Lease agent? thank you. i happened to buffed the surface with a wax and i read in easycomposites that there shouldnt be any wax prior to easy lease agent so i had to clean the part with acetone. now im at 2.coat of easy lease and it seems like doesnt leave anything behind and im abit anxious about the release. i hope its going to work out in the end  Thats part of what make it so good - virtually 0 build. To test it is working after you have applied 6-8 coats, try to stick a piece of masking tape to the part. It should come away very easily, with almost no resistance.
|
|
|
orhanyor
|
|
Group: Forum Members
Posts: 3,
Visits: 14
|
+x+x+xHello guys, newbie here  Recently i created my first negative mould and used up most of the epoxy gel coat on that. so im working on this very small negative mould as big as my hand. i just finished polishing the actual part's top surface that i should be spreading my gel coat on. The thing is i want to use the remaining epoxy gel coat on my next item and i dont have enough at the moment for the both parts. So is there an alternative to gelcoat that i can make with epoxy resin? I have some fumed silica, i was thinking may be i can use it to thicken the epoxy and use it instead of gel coat. has anybody tried it? my approach on my first mould was 2 coats of gel coat on top of the part. leave it to cure but when its still tacky i applied fiberglass with epoxy and then vacuum the whole thing. as a release agent i bought Easy-Lease Chemical Release Agent, PVA release agent, number 8 release wax and MANN ease release 200 spray i guess i have enough release agents but im not really sure which one works better. i read PVA is almost guaranteed so i used it in my first mould and i guess i brushed it too thick so it gave me abit of a problem during demoulding. Can i just use MANN spray as a release agent as it is very easy to use, is it reliable? Thanks Yes it does work, I just add a thix powder called Cabosil to get a good consistency. It takes a while to blend in well and you need to be sure it's not too thin as epoxy resins seem to separate/fisheye on release agents pretty easily. im thinking abit more thinner than a peanut butter consistency just enough to hold on vertical walls. when cured but still tacky i will lay some fiberglass and i hope its going to work. thank you for the response. have you tried MANN spray or Easy-Lease agent? thank you. i happened to buffed the surface with a wax and i read in easycomposites that there shouldnt be any wax prior to easy lease agent so i had to clean the part with acetone. now im at 2.coat of easy lease and it seems like doesnt leave anything behind and im abit anxious about the release. i hope its going to work out in the end 
|
|
|
Hanaldo
|
|
Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
+x+x+xHello guys, newbie here  Recently i created my first negative mould and used up most of the epoxy gel coat on that. so im working on this very small negative mould as big as my hand. i just finished polishing the actual part's top surface that i should be spreading my gel coat on. The thing is i want to use the remaining epoxy gel coat on my next item and i dont have enough at the moment for the both parts. So is there an alternative to gelcoat that i can make with epoxy resin? I have some fumed silica, i was thinking may be i can use it to thicken the epoxy and use it instead of gel coat. has anybody tried it? my approach on my first mould was 2 coats of gel coat on top of the part. leave it to cure but when its still tacky i applied fiberglass with epoxy and then vacuum the whole thing. as a release agent i bought Easy-Lease Chemical Release Agent, PVA release agent, number 8 release wax and MANN ease release 200 spray i guess i have enough release agents but im not really sure which one works better. i read PVA is almost guaranteed so i used it in my first mould and i guess i brushed it too thick so it gave me abit of a problem during demoulding. Can i just use MANN spray as a release agent as it is very easy to use, is it reliable? Thanks Yes it does work, I just add a thix powder called Cabosil to get a good consistency. It takes a while to blend in well and you need to be sure it's not too thin as epoxy resins seem to separate/fisheye on release agents pretty easily. im thinking abit more thinner than a peanut butter consistency just enough to hold on vertical walls. when cured but still tacky i will lay some fiberglass and i hope its going to work. thank you for the response. have you tried MANN spray or Easy-Lease agent? Don't use Mann release, it's really more of a casting release agent. Easylease is a superb release agent and is made for what you are doing. If you do 6-8 coats of Easylease with 15 minutes between each coat, parts with good draft should virtually fall out of the mould.
|
|
|
orhanyor
|
|
Group: Forum Members
Posts: 3,
Visits: 14
|
+x+xHello guys, newbie here  Recently i created my first negative mould and used up most of the epoxy gel coat on that. so im working on this very small negative mould as big as my hand. i just finished polishing the actual part's top surface that i should be spreading my gel coat on. The thing is i want to use the remaining epoxy gel coat on my next item and i dont have enough at the moment for the both parts. So is there an alternative to gelcoat that i can make with epoxy resin? I have some fumed silica, i was thinking may be i can use it to thicken the epoxy and use it instead of gel coat. has anybody tried it? my approach on my first mould was 2 coats of gel coat on top of the part. leave it to cure but when its still tacky i applied fiberglass with epoxy and then vacuum the whole thing. as a release agent i bought Easy-Lease Chemical Release Agent, PVA release agent, number 8 release wax and MANN ease release 200 spray i guess i have enough release agents but im not really sure which one works better. i read PVA is almost guaranteed so i used it in my first mould and i guess i brushed it too thick so it gave me abit of a problem during demoulding. Can i just use MANN spray as a release agent as it is very easy to use, is it reliable? Thanks Yes it does work, I just add a thix powder called Cabosil to get a good consistency. It takes a while to blend in well and you need to be sure it's not too thin as epoxy resins seem to separate/fisheye on release agents pretty easily. im thinking abit more thinner than a peanut butter consistency just enough to hold on vertical walls. when cured but still tacky i will lay some fiberglass and i hope its going to work. thank you for the response. have you tried MANN spray or Easy-Lease agent?
|
|
|
Fasta
|
|
Group: Forum Members
Posts: 468,
Visits: 3.5K
|
+xHello guys, newbie here  Recently i created my first negative mould and used up most of the epoxy gel coat on that. so im working on this very small negative mould as big as my hand. i just finished polishing the actual part's top surface that i should be spreading my gel coat on. The thing is i want to use the remaining epoxy gel coat on my next item and i dont have enough at the moment for the both parts. So is there an alternative to gelcoat that i can make with epoxy resin? I have some fumed silica, i was thinking may be i can use it to thicken the epoxy and use it instead of gel coat. has anybody tried it? my approach on my first mould was 2 coats of gel coat on top of the part. leave it to cure but when its still tacky i applied fiberglass with epoxy and then vacuum the whole thing. as a release agent i bought Easy-Lease Chemical Release Agent, PVA release agent, number 8 release wax and MANN ease release 200 spray i guess i have enough release agents but im not really sure which one works better. i read PVA is almost guaranteed so i used it in my first mould and i guess i brushed it too thick so it gave me abit of a problem during demoulding. Can i just use MANN spray as a release agent as it is very easy to use, is it reliable? Thanks Yes it does work, I just add a thix powder called Cabosil to get a good consistency. It takes a while to blend in well and you need to be sure it's not too thin as epoxy resins seem to separate/fisheye on release agents pretty easily.
|
|
|
orhanyor
|
|
Group: Forum Members
Posts: 3,
Visits: 14
|
Hello guys, newbie here  Recently i created my first negative mould and used up most of the epoxy gel coat on that. so im working on this very small negative mould as big as my hand. i just finished polishing the actual part's top surface that i should be spreading my gel coat on. The thing is i want to use the remaining epoxy gel coat on my next item and i dont have enough at the moment for the both parts. So is there an alternative to gelcoat that i can make with epoxy resin? I have some fumed silica, i was thinking may be i can use it to thicken the epoxy and use it instead of gel coat. has anybody tried it? my approach on my first mould was 2 coats of gel coat on top of the part. leave it to cure but when its still tacky i applied fiberglass with epoxy and then vacuum the whole thing. as a release agent i bought Easy-Lease Chemical Release Agent, PVA release agent, number 8 release wax and MANN ease release 200 spray i guess i have enough release agents but im not really sure which one works better. i read PVA is almost guaranteed so i used it in my first mould and i guess i brushed it too thick so it gave me abit of a problem during demoulding. Can i just use MANN spray as a release agent as it is very easy to use, is it reliable? Thanks
|
|
|