ni9eofse7en
n
ni9eofse7en
posted 5 Years Ago
ANSWER
HOT
Topic Details
n
Group: Forum Members
Posts: 4,
Visits: 11
Is Glasscast 50 or 10 heat resistant when cured, if so to what degree? Thanks in advance.
Reply
Like
5
Reply
ni9eofse7en
n
ni9eofse7en
posted 5 Years Ago
ANSWER
HOT
Post Details
n
Group: Forum Members
Posts: 4,
Visits: 11
Thank you Matt. Appreciated.
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Glasscast 50 or 10
ni9eofse7en
-
5 Years Ago
GlassCast 10 and 50 both have the same heat resistance, which is is about 65 degrees C. 65C is about as high as any epoxy can be temperature resistant to, without some kind a special heat treatment....
Matt (Staff)
-
5 Years Ago
Thank you Matt. Appreciated.
ni9eofse7en
-
5 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search