That postcuring process is a little bit risky always, the ramp has to be very very slow, fixing jig is always better. Like Lester said fix the bushings to the stable frame to be sure the final geometry will be ok, use slow ramp for longer time, remember the postcuring temperature has to be below the 3D core limit 5-10°C at least.
|